DESCRIPTION | IRAM | ASTM | DIN |
Rubber componed clasification | 113001 | D 2000 | |
Hardness Shore | 113003 | D 2240 | 53505 |
Traction Test | 113004 | D 412 | |
Thermic Aging | 113005 | D 573 | |
Compression test | 113010 | D 395 | |
Liquids Immersion | 113012 | D 471 | |
Rubber metal attachment | 113017 | D 429 | 53531 |
Abrasion (different methods) | 113016 | D 2228 / 1630 | 53516 |
RUBBER TESTS
– Traction
– Elongation resistance (incl. test tube extraction)
– Break resistance (die C – 90º angle)
– Compression Set
– Hardness Shore A
– Rheometric curve with interpretation
– 72 hours oil inmersion -minimum- (thermic aging)
Every 24 additional hours
– Volume change after immersion
– Abrasion according to DIN norm
– Polymeric identificación (including simple preparation)
– Carbon black content
– Acetone extract
– Contents of inorganic fillers
– Density
POLYMERIC USUALLY PROCESSED
Natural Rubber | SBR | VITON® |
HYPALON® | NEOPRENE® | EPDM |
Acrylic Nitrile | Butylic | Ebonite |
Silicone | Polyurethane |